Did you strip it with all the trim on ?

Nice leather !
Reply With Quote
  #2 (permalink)  
Old 23-02-11, 01:12 AM
Member
 
Join Date: Jan 2011
Location: Grand Cayman
Posts: 114
Default

Iam surprised how good the interior looks like.
And I admire you for the incredible work you have done so far.
In addition, I would like to mention, that you should check all areas of the body for thin aluminium, pinholes etc.
To check for thin aluminium, just gently press with a finger and see if the metal skin flexes. Pinholes - visual check.

Also, before you put on a fabulous new coat, check the underside for rust. It is better to have a competent company to repair the underside before any painjob.

Also, personally, I would not leave the Aluminium exposed too long.

And, before I forget, remove that rubber noisekilling strip before the paintjob.

Are the doors hagning straight and true? Hinges might need replacing if the pins are worn. Bristol have them.

The Window frames, seals and other bits will need to be replaced.

What colour did you have in mind?

Ah yes, one more tip:

If you clean all the lights with lukewarm water, dish washing liquid and a tooth brush (take apart first), then polish the outside surfaces, they will look like new, they will sparkle!
Lot of work (but nothing compared what you have done so far) but you will not regret it!

BTW, how is the engine? Sort out the resto of the engine before you paint the engine room.
Reply With Quote
  #3 (permalink)  
Old 23-02-11, 03:54 AM
Member
 
Join Date: May 2008
Location: Melbourne, Australia
Posts: 1,177
Default

Thanks for the pictures Mike. The interior looks quite good.

If you do decide to renovate the leather here is a link to some discussion on using the Woolies leather restoration kit.

If you work on any of the timber, be VERY careful when sanding off the old varnish because the veneer is quite thin and it's easy to sand through it!
Reply With Quote
  #4 (permalink)  
Old 23-02-11, 10:47 AM
Member
 
Join Date: Apr 2009
Location: York
Posts: 808
Default

Take a look at this leather restoration system as well -- great video instructions

Leather Dyes & Restoration
Reply With Quote
  #5 (permalink)  
Old 24-02-11, 02:17 PM
Member
 
Join Date: Jan 2011
Location: Grand Cayman
Posts: 114
Default

Quote:
Originally Posted by Kevin H View Post

If you work on any of the timber, be VERY careful when sanding off the old varnish because the veneer is quite thin and it's easy to sand through it!
Cannot agree more!

I used a Marine grade varnish, "International" brand.
Several layers, a light buff between the layers. Dustfree environment, like a bathroom.
(the wifes love it!)
Reply With Quote
  #6 (permalink)  
Old 24-02-11, 03:15 PM
Member
 
Join Date: Apr 2009
Location: York
Posts: 808
Default

This is the highest gloss toughest finish and can be done in one coat !

SP320 Solvent Free Clear Epoxy Resin System - mbfg.co.uk
Reply With Quote
  #7 (permalink)  
Old 24-02-11, 10:56 PM
Member
 
Join Date: May 2008
Location: Melbourne, Australia
Posts: 1,177
Default

Quote:
Originally Posted by GREG View Post
This is the highest gloss toughest finish and can be done in one coat !

SP320 Solvent Free Clear Epoxy Resin System - mbfg.co.uk
So why do they say;

"When used for coating wood, just a few coats will provide both protection and a depth of clarity that can only otherwise be achieved with many more coats of a conventional varnish."

Nevertheless, it sounds like good stuff!
Reply With Quote
  #8 (permalink)  
Old 25-02-11, 12:25 AM
Member
 
Join Date: Jan 2011
Location: Grand Cayman
Posts: 114
Default

What is the point of using a solvent free product?
No buzz - no joy!!

No need to polish the last layer. I used the marine varnish undiluted for maybe 4 layers, with a flattening with Wet and Dry paper after each coat. This way I achieved a perfectly flat surface, masking all undulations and irregularities in the wood panels.
For the last layer I diluted the laquer to thin it, and sieved it through a fine cloth to get rid of the little lumps.

It does not matter hich product you use, you need several layers. The thicker layer - the better "depth".

I forgot: If the veneer is cracked, it is usually better to give the job to a pro.
No need to go to a person that does cars, I would go to a person that does furniture restorations.
The same if I wanted to re-veneer the dashboard or the other bits.

In 1992 I veneered the dashboard and gearshift fascia on my 1991 AR Spider S4. I hated the crappy black plastic.
I used a veneer from the root section of Mahogany (proper Rainforest stuff in those days).
Lokked perfect untill I sold the car in 2004.
Marine varnish can take some water.

Last edited by Janne; 25-02-11 at 12:34 AM.
Reply With Quote
  #9 (permalink)  
Old 25-02-11, 09:43 AM
Member
 
Join Date: Apr 2009
Location: York
Posts: 808
Default

Quote:
Originally Posted by Kevin H View Post
So why do they say;

"When used for coating wood, just a few coats will provide both protection and a depth of clarity that can only otherwise be achieved with many more coats of a conventional varnish."

Nevertheless, it sounds like good stuff!
When it's applied on a flat surface, it can be applied thicker and one coat. It can be polished and it is the toughest product out there. I think it's the finish that is on modern car veneers ?
Reply With Quote
  #10 (permalink)  
Old 24-02-11, 10:54 PM
Member
 
Join Date: May 2008
Location: Melbourne, Australia
Posts: 1,177
Default

Quote:
Originally Posted by Janne View Post
Cannot agree more!

I used a Marine grade varnish, "International" brand.
Several layers, a light buff between the layers. Dustfree environment, like a bathroom.
(the wifes love it!)
I used Marine varnish as well (some Aussie brand), although I found it very hard to keep dust out, but I didn't do it in the bathroom!

I also tried polishing one section (glove box door) afterwards which didn't work out very well at all (not recommended!)

Perhaps an epoxy finish could be polished.
Reply With Quote
Reply

Tags
411, body work, exterior, filler, paint


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT. The time now is 03:48 PM.


This is the live site

Search Engine Friendly URLs by vBSEO 3.6.0 PL2